行业新闻

Yuming Valve Knowledge Hub | Common Materials for Valve Stems?

2023.11.22
yuming


The valve stem serves as a moving, load-bearing, and sealing component in the process of valve opening and closing. It is subject to impact and corrosion from the medium, as well as friction from the packing. Therefore, the selection of valve stem materials must ensure sufficient strength, excellent impact toughness, wear resistance, and corrosion resistance under specified temperatures. As a wear-prone part, the material chosen for the valve stem should also have favorable machining and heat treatment properties.



Copper Alloys

Typical grades: QA19-2, HPb59-1-1.

Suitable for low-pressure valves with nominal pressure ≤1.6 MPa and operating temperatures ≤200°C.

Carbon Steel

Typical grades: A5, 35 steel.

After nitriding treatment, these are used for low- and medium-pressure valves handling ammonia, water, steam, and other media with nominal pressure ≤2.5 MPa.

A5 steel is suitable for valves with temperatures ≤300°C.

35 steel is suitable for valves with temperatures ≤450°C.

Note: Practical application has shown that nitrided carbon steel valve stems do not perform well in corrosion resistance and should be avoided.

Alloy Steel

Typical grades: 40Cr, 38CrMoA1A, 20CrMo1V1A.

40Cr: After chrome plating, suitable for nominal pressure ≤32 MPa and operating temperatures ≤450°C, handling water, steam, and petroleum.

38CrMoA1A: After nitriding treatment, it can withstand pressures of 10 MPa at 540°C, commonly used in power station valves.

20CrMo1V1A: After nitriding treatment, it can withstand pressures of 14 MPa at 570°C, also commonly used in power station valves.

Stainless Steel

Typical grades: 2Cr13, 3Cr13, 1Cr17Ni2, 1Cr18Ni12Mo2Ti.

2Cr13, 3Cr13: Suitable for nominal pressure ≤32 MPa and operating temperatures ≤450°C for water, steam, and weakly corrosive media. The surface can be enhanced by chrome plating or high-frequency quenching.

1Cr17Ni2: Used in stainless steel and low-temperature valves, resistant to corrosive media.

1Cr18Ni9Ti, 1Cr18Ni12Mo2Ti: These stainless acid-resistant steels are used in high-temperature valves with nominal pressure ≤6.4 MPa and operating temperatures ≤600°C, or in low-temperature valves operating at ≤-100°C.

1Cr18Ni9Ti: Resistant to nitric acid and other corrosive media.

1Cr18Ni12Mo2Ti: Resistant to acetic acid and other corrosive media.

For high-temperature applications, both materials can be nitrided to enhance anti-wear performance.

Bearing Chrome Steel

Grade: GCr15.

Used in ultra-high-pressure valves with nominal pressure ≤300 MPa and operating temperatures ≤300°C.

In addition to the materials listed above, valve stems may also be made from 4Cr10Si2Mo martensitic heat-resistant steel, 4Cr14Ni14W2Mo austenitic heat-resistant steel, and other specialized alloys depending on specific requirements.